Airless Tires Near Me 178x50mm
1. The Parameters of Airless Tires 178x50mm
Size
(inch)
Diameter
(mm)
Width
(mm)
Weight
(g)
Bearing/Keyway
(mm)
Hub Length
(mm)
Item NO.
178x50
178+/-3
50 ±1.5
12
44.1
2. Applications of Airless Tires of 7 Inch
With the superior performance in the aspects of inflation free, anti- puncture, flat free, good cushioning maintenance free and high security etc., it is widely used in the following field:
Manual Wheelchairs
Power Wheelchairs
Mobility Scooters
Robots
Sweepers
Mowers
Ariel Platforms
And more
3. Analysis of PU Solid Tire Production Process
Process principle: the production process of Pu foamed tire mainly consists of evenly mixing PU materials (component A and component B) in the state of centrifugal rotation, pouring into the
mold, foaming and curing through chemical reaction.
A. PU material mixing;
The mixing mode of component A and component B is delivered to the pouring gun head by the low-pressure pouring machine through the precision metering pump, and the mechanical mixing is
carried out under the rotating speed of 4500 ~ 5000r / min to make the materials of component A and component B mixed evenly.
B. PU material filling into the mold;
The mold temperature is assisted by electric heating, and the mold temperature is controlled at 45 ~ 55 ℃. Before filling, the mold needs to be cleaned, then sprayed with release agent, and finally
closed the mold and filled with PU material.
C. Control of PU filling time
The filling time of the product is set to 4.5 ~ 5.5 seconds. During the production process, fine adjustment is made according to the appearance of tire production.
The filling time is set on the PLC control panel on the low-pressure machine.
D. Control of material temperature
The Material temperature is controlled by the material temperature control system of the low-pressure filling machine, and the material temperature of component A
and component B is controlled at 50 + / - 5 ℃
E. Control of pu tire demoulding time
The best demoulding time of the product is 5 minutes, which is timed by a timer. The early demoulding time will affect the appearance of the product, and it is easy to stick
the mold.
F. Solid tire trimming
The pu material injection port and non air hole burr with the trimming tool, and remove the burr at the parting line at the same time.
G. PU solid tire cooling
The chemical reaction of PU material is a complex reaction process. After demoulding, the moisture in the air and trace chemicals in the material will continue to react and solidify with component B. therefore, the PU tire must be placed for 48 hours after demoulding to fully mature the product and achieve the best performance before the tire pressing assembly process can be carried out. At the same time, the chemical reaction of polyurethane material is an exothermic reaction. After demoulding, the central temperature of the tire product is still about 80 ℃, and the tire surface temperature is still about 50 ℃ (the specific situation will vary greatly according to the temperature in winter or summer). The product needs to be cooled naturally after molding to further mature the PU material. Pay attention to the pressure marks and other phenomena during the placement of PU products.